SA 335 gr P11 Cyfansoddiad Cemegol Pibell Ddi-dor

C, % Mn, % P, % S, % Si, % Cr, % Mo, %
0.015 uchafswm 0.30-0.60 0.025 uchafswm 0.025 uchafswm 0.50 uchafswm 4.00-6.00 0.45-0.65

 

Priodweddau Pibellau Dur ASTM A335 P11

Cryfder Tynnol, MPa Cryfder Cynnyrch, MPa Elongation, %
415 mun 205 mun 30 mun

A335 P11 Steel Pipe

Siart Tynnol o P11 Alloy Steel Pipe Welded

  Pibell Ddi-dor  
  P5 P9 P11 P22 P91
Cryfder Tynnol, lleiafswm., psi          
ksi 60 60 60 60 85
Mpa 415 415 415 415 585
Yield Strength, lleiafswm., psi          
ksi 30 30 30 30 60
Mpa 205 205 205 205 415