Pibell Dur Pwysedd Uchel ASTM A335
Dec 04, 2025
Beth yw Deunydd A335
Mae pibell ddur di-dor ASTM A335 yn safon a sefydlwyd gan Gymdeithas Profi a Deunyddiau America (ASTM) i reoleiddio pibellau dur aloi ferritig di-dor ar gyfer gwasanaeth tymheredd uchel. Mae'r safon hon yn cwmpasu gwahanol raddau, megis P1, P2, P5, P9, P11, P22, P91, ac ati, pob un â chyfansoddiadau cemegol penodol a nodweddion perfformiad i gwrdd â gofynion gwahanol amgylcheddau tymheredd uchel a gwasgedd uchel. Defnyddir pibellau dur di-dor ASTM A335 yn bennaf mewn systemau pibellau tymheredd uchel a gwasgedd uchel mewn diwydiannau fel cynhyrchu pŵer a phetrocemegol. Yn y sector pŵer, maent yn cael eu cyflogi'n gyffredin mewn cydrannau fel uwch-gynheswyr boeleri, ailgynheswyr, a phrif bibellau stêm. Rhaid i'r cydrannau hyn wrthsefyll effeithiau stêm pwysedd uchel a phwysau uchel, sy'n gofyn am gryfder tymheredd uchel eithriadol, ymwrthedd ocsideiddio, a gwrthiant ymgripiad o ddeunydd y bibell.
Manyleb A335 Alloy Steel Pipe
| Enw Cynnyrch | Pibell Dur aloi |
| Deunydd | Dur aloi |
| Hyd Pibell | Hyd Hap Sengl a Hyd Ar Hap dwbl.SRL:3M-5.8M DRL:10-11.8M neu Fel y gofynnwyd hyd gan gleientiaid |
| Maint | Maint 1/4" i 24" Diamedr y tu allan 13.7 mm i 609.6 mm |
| Trwch wal | SCH10, SCH20, SCH30, STD, SCH40, SCH60, SCH80, SCH100 SCH120, SCH160, XS, XXS |
| Safonol |
ASTM A 335 Gradd P1, P2, P5, P9, P9A, P11, P22.ASTM A213 T1B, T1, T2, T5, T9, T9A, T11, T12, T22.A199 T5, T9, T11, T22. DIN 17175 15 Mo 3, 13 Cr Mo 44, 10 Cr Mo 910, 14 Mo V 63, X 20 Cr Mo V 121 . JIS G3458/G3462/3467 |
| Ceisiadau | Pibell 1.Fluid 2. Power Planhigion 3. pibell strwythur 4. tiwb boeler pwysedd uchel ac isel 5. tiwbiau dur di-dor ar gyfer cracio petrolewm 6. pibell cwndid 7. Fferyllol pibellau sgaffaldiau ac adeiladu llongau ac ati |
| Tystysgrif | ISO/PED/TUV/SGS/LR/BV |
| Prif Farchnad | Asia, y Dwyrain Canol, Ewrop, America, Affrica, Awstralia, ac ati |
Pibell Dur Aloi Di-dor A335 ar gyfer gwasanaeth tymheredd uchel Cyfansoddiad Cemegol (%):
|
Gradd |
Dynodiad UNS |
Cyfansoddiad, % |
|||||||
|
Carbon |
Manganîs |
Ffosfforws, |
Sylffwr |
Silicon |
Cromiwm |
Molybdenwm |
Eraill |
||
|
max |
max |
||||||||
|
P1 |
K11522 |
0.10–0.20 |
0.30–0.80 |
0.025 |
0.025 |
0.10–0.50 |
- |
0.44–0.65 |
- |
|
P2 |
K11547 |
0.10–0.20 |
0.30–0.61 |
0.025 |
0.025 |
0.10–0.30 |
0.50–0.81 |
0.44–0.65 |
- |
|
P5 |
K41545 |
0.15 uchafswm |
0.30–0.60 |
0.025 |
0.025 |
0.50 uchafswm |
4.00–6.00 |
0.45–0.65 |
- |
|
P9 |
S50400 |
0.15 uchafswm |
0.30–0.60 |
0.025 |
0.025 |
0.25–1.00 |
8.00–10.00 |
0.90–1.10 |
- |
|
P11 |
K11597 |
0.05–0.15 |
0.30–0.60 |
0.025 |
0.025 |
0.50–1.00 |
1.00–1.50 |
0.44–0.65 |
- |
|
P12 |
K11562 |
0.05–0.15 |
0.30–0.61 |
0.025 |
0.025 |
0.50 uchafswm |
0.80–1.25 |
0.44–0.65 |
- |
|
P15 |
K11578 |
0.05–0.15 |
0.30–0.60 |
0.025 |
0.025 |
1.15–1.65 |
- |
0.44–0.65 |
- |
|
P21 |
K31545 |
0.05–0.15 |
0.30–0.60 |
0.025 |
0.025 |
0.50 uchafswm |
2.65–3.35 |
0.80–1.06 |
- |
|
P22 |
K21590 |
0.05–0.15 |
0.30–0.60 |
0.025 |
0.025 |
0.50 uchafswm |
1.90–2.60 |
0.87–1.13 |
- |
|
P23 |
K41650 |
0.04–0.10 |
0.10–0.60 |
0.03 |
0.01 |
0.50 uchafswm |
1.90–2.60 |
0.05–0.30 |
V 0.20–0.30 |
|
Cb 0.02–0.08 |
|||||||||
|
B 0.0005–0.006 |
|||||||||
|
N 0.030 uchafswm |
|||||||||
|
Al 0.030 uchafswm |
|||||||||
|
W 1.45–1.75 |
|||||||||
|
P91 |
K91560 |
0.08–0.12 |
0.30–0.60 |
0.02 |
0.01 |
0.20–0.50 |
8.00–9.50 |
0.85–1.05 |
V 0.18–0.25 |
|
N 0.030–0.070 |
|||||||||
|
Ni 0.40 uchafswm |
|||||||||
|
Al 0.04 max |
|||||||||
|
Cb 0.06–0.10 |
|||||||||
|
P92 |
K92460 |
0.07–0.13 |
0.30–0.60 |
0.02 |
0.01 |
0.50 uchafswm |
8.50–9.50 |
0.30–0.60 |
V 0.15–0.25 |
|
N 0.03–0.07 |
|||||||||
|
Ni 0.40 uchafswm |
|||||||||
|
Al 0.04 max |
|||||||||
|
Cb 0.04–0.09 |
|||||||||
|
W 1.5–2.00 |
|||||||||
|
B 0.001–0.006 |
|||||||||
A335 Cr-Pibell ddur aloi Mo Priodweddau Mecanyddol:

Technoleg Triniaeth Gwres
Trwy brosesau fel anelio llawn, normaleiddio gyda thymheru, mae straen gweddilliol o brosesu yn cael ei ddileu a strwythur grawn yn cael ei fireinio. Mae camau allweddol yn cynnwys:
Gwresogi i 900-950 gradd ac yna oeri aer
Tymheru ar 650-700 gradd
Rheolaeth lem ar gyfraddau gwresogi ac oeri
System Arolygu
Rhaid i bob swp basio:
Dadansoddiad sbectrosgopig i wirio cyfansoddiad cemegol
Profion tynnol ar gyfer priodweddau mecanyddol
Profi cerrynt uwchsonig / eddy i ganfod diffygion mewnol
Profi hydrostatig i ddilysu perfformiad selio

Pecynnu a llongau