Pibell ASTM A178 mewn Stoc

Sep 07, 2023

Disgrifiad o'r Cynnyrch

Mae pibellau ASTM A178 yn bibellau dur carbon a charbon manganîs ERW a ddefnyddir mewn boeleri, ffliwiau boeleri, ac uwchgynhesyddion. Mae gan ASTM A178 A178 gradd A (dur carbon isel), A178 gradd C (dur carbon canolig), ac A178 gradd D (dur carbon). ) dur manganîs).

Pibell ASTM A178 mewn Manyleb Stoc

Enw Cynnyrch

Pibell ASTM A178 mewn Stoc

Diamedr allanol

14mm-720mm

Deunydd

GB10#,20,#35,40#,45#,16Mn,35Mn2,40Mn2,45Mn2,35SiMn,42SiMn,40Cr,Q345,Q355,Q390,20MnG,25MnG,15GMoG,25CMoG,25CMoG,25CMoG,25CMoG,25CMoG,20CMoG,20CMoG,20CMoG,20CMoG,20MnG 12Cr1MoVG, 10MoWVNb, 12CrMo,15CrMo,1Cr5Mo,12Cr2Mo,37Mo,30CrMo,35CrMo,34CrMo4,T/P5,T/P9,DZ40,DZ50,DZ55,DZ60,STM-R780

ASTM 1010,1012,1020,1035,1045,4130,4140,A53 Gr.A,A53 Gr.B,A53M,A36,A106 Gr.A/Gr.B
ASEM SA106A/B/C, SA192, T1/T1a, SA210A1/C, T/P2, T/P11, T/P12,T/P22,T23,T24,T/P91

EN P195/235/265GH,16Mo3,13CrMo4-5},13CrMo9-10,15NiCuMoNb5-6-4 St35.8, St45.8,15Mo3,13CrMo44,10CrMo910
JIS S10C/S20C/S35C/S45C/Q195/Q215/Q235/Q255/Q275/Q290

API 5L Gr.B
............

Safonol

GB3094,8162,8163,3639,3087,6479,5310,9948,6479,17396 ,GB/T 17396 ,Q/OHAD010-1998 ,YB/T 5052 Q/OHAD{{B1/T}, YB/T 5035 Q/OHAD001-1997, Q/OHAD015-2008, Q/OHAD002-2010

ASTM A53, A179, A192, A106, ASTM A36, A519, A213, A335

ASEM SA106/SA192/SA209/SA210/SA213/SA335

JIS STPG370, STPT370, STB240

DIN 17175/2391-2

EN 10216% 2f10210

API 5L

............

Goddefgarwch safonol dyddiol

od: +-1%, pwysau: +-10%

Gwirio

ISO BV SGS SVG

Pecyn

Pacio teilyngdod môr safonol neu yn ôl yr angen.

MOQ

5 tunnell fetrig, derbynnir archeb sampl

Amser cludo

7-10 diwrnod gwaith ar ôl derbyn blaendal neu lythyr credyd

Dull talu

30%TT+70%TT/LC etc

Disgrifiwch

Arwyneb: paentio, gorchuddio AG, galfanedig

Y cais

1. Piblinell trawsyrru hylif pwysedd canolig ac isel

2. Y casin
3. y tiwb boeler
4. diwydiant olew a nwy
5. diwydiant cemegol
6. diwydiant pŵer

Mantais

Pris 1.Reasonable, o ansawdd da

Stocrestr 2.Sufficient, cyflenwi cyflym
Profiad allforio 3.Rich a gwasanaeth diffuant
Anfonwyr cludo nwyddau 4.Reliable

Pipe ASTM A178 in Stock

 

ASTM A178 Cyfansoddiad Cemegol
Gradd Carbon Manganîs Ffosfforws Sylffwr Silicon
ASTM A178 Gr A 0.06% - 0.18% 0.27% - 0.63% 0.035% Uchafswm 0.035% Uchafswm -
ASTM A178 G C 0.35% Uchafswm 0.80% Uchafswm 0.035% Uchafswm 0.035% Uchafswm -
ASTM A178 G D 0.27% Uchafswm 1.00% - 1.50% 0.30% Uchafswm 0.015% Uchafswm 0.10% Munud

 

Priodweddau Mecanyddol ASTM A178
Gradd P # Cryfder Tynnol Cnwd Caledwch Uchaf Gwirio Stocrestr
ASTM A178 Gr A/SA178A P 1 ks: 47 MPa: 325 ks: 26 MPa: 180 77 HRB (Rockwell B) A178 Gr A Stocrestr
ASTM A178 Gr C/SA178C P 1 ks: 60 MPa: 415 ks: 37 MPa: 255 79 HRB (Rockwell B) A178 Rhestr Gr C
ASTM A178 Gr D/SA178D P 1 ks: 70 MPa: 485 ks: 40 MPa: 275 77 HRB (Rockwell B) A178 Rhestr Gr D