A335 Pibell Ddi-dor Carbon Wedi'i Dynnu'n Oer
Mae ASTM A335 yn cwmpasu "pibell ddur aloi isel, hynny yw, pibell â chyfanswm o lai na 5% o elfennau aloi. Mae ychwanegu cyfrannau uwch o elfennau aloi, megis nicel a chromiwm, yn trawsnewid y dur yn aloion datblygedig fel dur di-staen, dur deublyg, a thu hwnt.
A335 Cyflenwr Pibell Di-dor Carbon Wedi'i Dynnu'n Oer-GNEE
Pibell Dur Di-dor aloi A335
Defnyddir pibellau dur aloi yn bennaf mewn pibellau ac offer pwysedd uchel a thymheredd uchel fel gweithfeydd pŵer, ynni niwclear, boeleri pwysedd uchel, uwchgynhesyddion tymheredd uchel ac ailgynheswyr. Maent wedi'u gwneud o ddur carbon o ansawdd uchel, dur strwythurol aloi a dur di-staen sy'n gwrthsefyll gwres. , gan ddefnyddio rholio poeth (allwthio, ehangu diamedr) neu rolio oer (arlunio).
| maint | 1/2"—24" (DN15-600) |
| trwch | SCH10, SCH20, SCH30, STD, SCH40, SCH60, XS, SCH80, SCH100, SCH120, SCH140, SCH160, XXS, DIN, JIS trwch safonol |
| hyd | Sefydlog: 3.0 , 5.8 , 5.85 , 5.9 , 6.0 ,11.8 , 12.0m. Hyd ar hap: 5-12m |
| safonol | ASTM A53, A106, API 5L, ASME B36.10M-1996DIN1626, DIN1629, DIN17175, DIN 2448JIS G3452, JIS G3454, JIS G3455, JIS G3456, JISJ G33546, |
| Deunydd | C235, 20#, Q345A53B, A106B, API 5L B, X42,X46,X52,X60, X65ST37.0,ST35.8,St37.2,St35.4/8,St42,St45,St52, St52.4STP G38, STP G42, STPT42, STB42, STS42, STPT49, STS49 |
| defnydd | Piblinell hylif pwysedd canolig ac isel, boeler, diwydiant olew a nwy, drilio, diwydiant cemegol, diwydiant pŵer, adeiladu llongau, offer gwrtaith a phiblinell, strwythur, petrocemegol, diwydiant fferyllol |
| wyneb | Paent du, farnais, olew gwrth-rhwd, galfanedig poeth, galfanedig oer, 3PE, ac ati. |
| Pecyn | Gorchudd plastig ar y ddau ben, lletwad, bag wedi'i wehyddu neu yn unol â chais y cwsmer |
| Ardystiad | ISO9001, SGS, BV, ac ati |
A335 Cyfansoddiad Cemegol Pibell
| ASTM A335 Dur aloi isel (Graddau) |
UNS cyfatebol |
C Llai na neu'n hafal i | Mn | P Llai na neu hafal i | S Llai na neu'n hafal i | Si Llai na neu hafal i | Cr | Mo |
| P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
| P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
| P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
| P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
| P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
| P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
| P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
| P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
| P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
| P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
| P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
| P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
| P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
Priodweddau Mecanyddol Pibell Dur Alloy Isel A335
| Pibell Aloi Isel A335 | Rhif UNS | Cryfder Cynnyrch ksi | Cryfder Tynnol ksi | Elongation % | Rockwell | Brinell |
| P1 | K11522 | 30 | 55 | 30 | – | – |
| P2 | K11547 | 30 | 55 | 30 | – | – |
| P5 | K41545 | 40 | 70 | 30 | – | 207 uchafswm |
| P9 | S50400 | 30 | 60 | 30 | – | – |
| P11 | K11597 | 30 | 60 | 20 | – | – |
| P12 | K11562 | 32 | 60 | 30 | – | 174 uchafswm |
| P22 | K21590 | 30 | 60 | 30 | – | – |
| P91 | K91560 | 60 | 85 | 20 | – | – |
Pibell Dur aloi A335

FAQ:
1. Pam ein dewis ni?
Mae ein cwmni wedi bod mewn busnes metel am fwy na deng mlynedd (allforio am fwy na 3 blynedd), rydym yn brofiadol yn rhyngwladol, yn broffesiynol, a gallwn ddarparu amrywiaeth o gynhyrchion dur o ansawdd uchel i'n cleientiaid.
2. Gall ddarparu gwasanaeth OEM/ODM?
Oes. Mae croeso i chi gysylltu â ni am fwy o fanylion trafod.
3. A allwn ni ymweld â'ch ffatri?
Croeso cynnes. Unwaith y bydd gennym eich amserlen, byddwn yn trefnu i'r tîm gwerthu proffesiynol fynd ar drywydd eich achos.
4. Allwch chi ddarparu sampl?