310S Stainless Steel Seamless Pipe
310S Stainless Steel Seamless Pipe
1/2
<< /span>
>

Pibell Di-dor Dur Di-staen 310S

Mae ein pibell di-dor dur di-staen 310S yn ddatrysiad pibellau o ansawdd uchel, wedi'i ddylunio'n fanwl, sydd wedi'i gynllunio i fodloni gofynion llym ystod eang o gymwysiadau diwydiannol.

 

Pibell Di-dor Dur Di-staen 310S

Mae 310S yn ddur di-staen cromiwm-nicel austenitig gydag ymwrthedd ocsideiddio da a gwrthiant cyrydiad. Oherwydd y cynnwys uchel o gromiwm a nicel, mae gan 310S gryfder ymgripiad gwell, gall barhau i weithio ar dymheredd uchel, ac mae ganddo wrthwynebiad da i gyrydiad. Perfformiad tymheredd uchel.

Manylion Pibell Di-dor Dur Di-staen 310S

Enw Cynnyrch

Pibell Dur Di-staen

Gradd

201, 304, 316L, 310S, 2205 2507, ac ati.

Safonol

AISI, ASTM, DIN, JIS, BS, DS

Hyd

1000-6000 mm

Trwch

0.4-30 mm

Arwyneb

sgleinio, llinell gwallt, ac ati

Pecyn

Pacio Safonol Teilwng i'r Môr neu Wedi'i Addasu

Amser dosbarthu

8-14 diwrnod yn amodol ar ofynion a maint y cwsmer

310S Stainless Steel Seamless Pipe

 

 

CYFANSODDIAD CEMEGOL PIBELLAU A TIWBIAU UNS S31008:

Gradd C Mn Si P S Cr Mo Ni N
310S 0.08 uchafswm 2 uchafswm 1.50 uchafswm 0.045 uchafswm 0.03 uchafswm 24 – 26 - 19 – 22 -

 

310S PIBELLAU A TIWB EIDDO MECANYDDOL A FFISEGOL:

Dwysedd 8.0 g/cm3
Ymdoddbwynt 1454 gradd (2650 gradd F)
Cryfder Tynnol Psi – 75000 , MPa – 515
Cryfder Cynnyrch (0.2% Offset) Psi – 30000, MPa – 205
Ymuniad 35 %

 

Amrediad Maint Pibellau Dur Di-staen 310S
NPS OD SCH 5S SCH 10S SCH 40S SCH 80S
1/4 13.72 1.65 2.24 3.02
3/8 17.15 1.65 2.31 3.2
1/2 21.34 1.65 2.11 2.77 3.73
3/4 26.67 1.65 2.11 2.87 3.91
1 33.4 1.65 2.77 3.38 4.55
1.25 42.16 1.65 2.77 3.56 4.85
1.5 48.26 1.65 2.77 3.68 5.08
2 60.33 1.65 2.77 3.91 5.54
2.5 73.03 2.11 3.05 5.16 7.01
3 88.9 2.11 3.05 5.49 7.62
3.5 101.6 2.11 3.05 5.74 8.08
4 114.3 2.11 3.05 6.02 8.56
5 141.3 2.77 3.4 6.55 9.53
6 168.28 2.77 3.4 7.11 10.97
8 219.08 2.77 3.76 8.18 12.7
10 273.05 3.4 4.19 9.27 12.7
12 323.85 3.96 4.57 9.53 12.7
14 355.6 3.96 4.78 9.53 12.7
16 406.4 4.19 4.78 9.53 12.7
18 457.2 4.19 4.78 9.53 12.7
20 508 4.78 5.54 9.53 12.7
22 558.8 4.78 5.54
24 609.6 5.54 6.35 9.53 12.7
26 660.4
28 711.2
30 762 6.35 7.92

 

 

EIN TÎM

310S Stainless Steel Seamless Pipe

EIN FFATRI

310S Stainless Steel Seamless Pipe

 

Tagiau poblogaidd: 310au dur gwrthstaen bibell di-dor, Tsieina 310au dur gwrthstaen bibell di-dor gweithgynhyrchwyr, cyflenwyr, ffatri

Anfon ymchwiliad

(0/10)

clearall