  PSL/ Lefel Manyleb Cynnyrch
Mathau Prawf API 5L Gradd BPSL 2
Profi swynol Mendentery ar gyfer API 5L Grb Pipe a graddau eraill
Ardystiad deunydd PSL2 API 5L Gradd B gofynnol (SR 15.1)
NDT ar gyfer L245 Gradd B Pibell Ddi-dor Angen SR4
Olrheiniadwyedd Gellir ei olrhain ar ôl cwblhau profion API5LB (SR 15.2) yn orfodol
Carbon Steel API 5L Gr B Piblinell Prawf Hydrostatig Mendentery

 

10-10-25

 

Gradd B PSL1 PSL2
Cryfder Cynnyrch Isaf: 35% 2c000 psi 35% 2c000 psi
Cryfder Cynnyrch Uchaf: Dim 65% 2c000 psi
Cryfder Tynnol Isaf: 60% 2c000 psi 60% 2c000 psi
Cryfder Tynnol Uchaf: Dim 110% 2c000 psi

 