| Maint OD, Inches |
BW Ga. |
Wal Rhag-Yn. |
ID | Pwysau Lbs/Ft. |
| 1/8 | 22 | 0.028 | 0.069 | 0.0290 |
| 20 | 0.035 | 0.055 | 0.0336 | |
| 3/16 | 22 | 0.028 | 0.131 | 0.0478 |
| 1/4 | 25 | 0.020 | 0.210 | 0.0491 |
| 22 | 0.028 | 0.194 | 0.0664 | |
| 21 | 0.032 | 0.187 | 0.0745 | |
| 20 | 0.035 | 0.180 | 0.0804 | |
| 18 | 0.049 | 0.152 | 0.1052 | |
| 16 | 0.065 | 0.120 | 0.1284 | |
| 5/16 | 20 | 0.035 | 0.242 | 0.1039 |
| 18 | 0.049 | 0.214 | 0.1382 | |
| 16 | 0.065 | 0.182 | 0.1722 | |
| 3/8 | 22 | 0.028 | 0.319 | 0.1038 |
| 20 | 0.035 | 0.305 | 0.1271 | |
| 18 | 0.049 | 0.277 | 0.1706 | |
| 16 | 0.065 | 0.245 | 0.2152 | |
| 7/16 | 18 | 0.049 | 0.340 | 0.2036 |
| 1/2 | 25 | 0.020 | 0.460 | 0.1025 |
| 20 | 0.035 | 0.430 | 0.1738 | |
| 18 | 0.049 | 0.402 | 0.2360 | |
| 16 | 0.065 | 0.370 | 0.3020 | |
| 5/8 | 20 | 0.035 | 0.555 | 0.2205 |
| 18 | 0.049 | 0.527 | 0.3014 | |
| 16 | 0.065 | 0.495 | 0.3888 | |
| 3/4 | 20 | 0.035 | 0.680 | 0.2673 |
| 18 | 0.049 | 0.652 | 0.3668 | |
| 16 | 0.065 | 0.620 | 0.4755 | |
| 14 | 0.083 | 0.584 | 0.5913 | |
| 7/8 | 18 | 0.049 | 0.777 | 0.4323 |
| 16 | 0.065 | 0.745 | 0.5623 | |
| 11 | 0.120 | 0.635 | 0.9676 | |
| 1 | 20 | 0.035 | 0.930 | 0.3607 |
| 18 | 0.049 | 0.902 | 0.4977 | |
| 16 | 0.065 | 0.870 | 0.6491 | |
| 14 | 0.083 | 0.834 | 0.8129 | |
| 11 | 0.120 | 0.760 | 1.1278 | |
| 1-1/4 | 11 | 0.120 | 1.010 | 1.4480 |
Tiwb Dur Di-staen 316L